Type :
HZ-PF
Character:
White powder,granularity<20 mesh, Moisture <0.5%
Applicate
scope:
Non-high mg al alloy
Recommend
dosage:
Use level 2~
Refining temperature: 700º C~750º C.
Use method:
Adding refining flux of required amount into refining tank and cover it
properly, turn on the switch of refining tank and connect nitrogen gas. When
refining flux is spraying out of refining iron tube, insert it into the furnace
and move all around inside evenly for 2 or 3 times. When powder inside the tank
is sprayed completely, first draw out the refining tube out of aluminium
liquid, and then switch off nitrogen gas.
Main features:
1. High efficiency, 100% efficient composition.
2. Strong purifying capacity up to domestic advanced level.
3. Less pollution, small consumption and low cost.
Packaging and storage:
2.5~10kg/ bag,20~50kg/carton or box. Be stored in a dry and ventilated place.